Quality defect & treating methods of dry lamination

2016-09-21 09:55:24 | 高齢社会
A、Phenomenon:
There are many scattered spots on the surface of lamination film,especially on the metallized products or light ink printed products.It appears dusky color when serious.
2、Reasons and strategies
1)Lack of coating—— Adding coating
2)Levelling property of cementing compound is poor.——Using better levelling property cementing compound,which contains high solid and low viscosity.
3)The surface tension force of basic film is too small——redealing with basic film and improving the surface tension force.
4)Too much solvent residue——adjusting dull and dry workmanship
5) Changing the coating method is also a way to deal with hickie.